The 304 vs 202 stainless steel kitchen equipment question comes down to one metal: nickel. The amount of nickel decides how well the steel survives salt, water and acid. Both grades look the same once polished. So a quote can name one grade while the table is built from the other. This guide covers the metal mix, the price gap, the tests that work and the ones that don't. It also shows where each grade fits, from a 100-cover hotel kitchen to a chaat thela in Indore.

SS 304

₹180–220 per kg

18–20% chromium and 8–10.5% nickel. The standard food-industry grade for wet, salty work.

SS 202

₹140–170 per kg

17–19% chromium, 4–6% nickel and 7.5–10% manganese. Less rust resistance in wet use.

Sheet and coil price ranges: OfBusiness, undated, read 15 Nov 2026. Metal mix: ASTM (American Society for Testing and Materials) ranges via ISSF (2005) and ASSDA (2013).

What are SS 304 and SS 202 stainless steel?

A stainless steel grade is a fixed recipe of metals. Chromium is the metal that stops rust. It forms a thin, invisible layer on the surface. Nickel makes that layer stronger and the steel easier to shape. Manganese is a cheaper metal that can take part of nickel's place.

SS 304 has 18–20% chromium and 8–10.5% nickel. It is the standard grade of the food industry (Euro Inox food and beverage guide). SS 202 has 17–19% chromium, only 4–6% nickel and 7.5–10% manganese. The manganese replaces part of the nickel to cut cost. Sources: International Stainless Steel Forum (ISSF, 2005) and Australian Stainless Steel Development Association (ASSDA, 2013).

Both grades are austenitic. This is a steel family that is not magnetic when annealed, or softened by heat after rolling. On a finished table the two look the same. The difference is inside the metal. 202 has less chromium and less nickel, so it resists corrosion (rust, stains and pitting) less. Even lower-nickel grades exist. Grade 201 has 3.5–5.5% nickel. The J4 type has about 1% nickel and 15–16% chromium (ASSDA, 2013).

ASTM composition ranges (ISSF 2005; ASSDA 2013)
ElementSS 304SS 202
Chromium18–20%17–19%
Nickel8–10.5%4–6%
Manganesemax 2%7.5–10%
Carbonmax 0.08%max 0.15%
Nitrogenmax 0.10%max 0.25%

For a small owner, the grade question may cover one table or one counter. For a hotel, it runs through a whole commercial kitchen equipment range, from work tables and sinks to burner ranges and display counters.

How do 304, 202, 430 and 316 compare for kitchen equipment?

SS 304 is the all-round grade for food zones. 202 is a cheaper grade for dry areas. 430 is a magnetic grade for outer panels. 316 is the upgrade for salt, brine and sea air. The two tables below compare the four grades in pairs. Chromium alone does not decide how a grade performs. Nickel, manganese and molybdenum (a metal that helps steel resist salt) matter too.

Pitting is rust that eats small, deep holes into the surface. PREN (Pitting Resistance Equivalent Number) is a score that ranks grades against pitting. It adds the chromium percentage, 3.3 times the molybdenum and 16 times the nitrogen. A higher score means better resistance. The score only ranks grades; it does not predict how many years steel lasts. Sources: steel maker Outokumpu and the International Molybdenum Association (IMOA). No published PREN exists for 202, so its figure below is an estimate from the formula.

Grade comparison, part 1: 304 and 202
PropertySS 304SS 202
Nickel8–10.5%4–6%
PREN≈19≈17–21 (estimate)
MagneticNo; slightly when cold-workedNo; slightly when cold-worked
Rust resistanceGood indoors; food-industry standardLower; pitting and tea staining in wet, salty use
Sheet price₹180–220 per kg₹140–170 per kg
Best usePrep tops, sinks, dishwash, rangesDry frames, undershelves, panels away from water
Grade comparison, part 2: 430 and 316
PropertySS 430SS 316
Nickelmax 0.75%10–14%, plus 2–3% molybdenum
PREN≈16.5–18≈24
MagneticYes, stronglyNo
Rust resistanceFair indoors in dry areasBest; salt, brine and coastal air
Sheet priceNo current price found₹280–350 per kg
Best useOuter panels, appliance bodies, doorsCoastal, pickle, brine and seafood kitchens

All four grades carry 16–20% chromium. Metal mix comes from ISSF (2005), ASSDA (2013), Jindal Stainless (Jan 2025) and Euro Inox. PREN comes from published grade tables. Prices are OfBusiness ranges read in November 2026.

Does 202 stainless steel rust in a commercial kitchen?

Yes, in wet and salty conditions 202 rusts and stains more easily than 304. It holds up in dry indoor use. "200-series" means the low-nickel family that includes 201 and 202. In salt-spray tests run for 575 hours, 304 stayed sound. 200-series samples with 4% and 1% nickel corroded significantly (ISSF, 2005). A crevice is a tight gap, such as under a bolt or inside a joint. In acidic crevice tests, the 1%-nickel grade dissolved about 10 times faster than 304.

ASSDA rates chromium-manganese grades as generally less corrosion resistant than chromium-nickel grades. It reports serious corrosion failures and tea staining in Asia where grades were mixed up (ASSDA, 2013). Tea staining is a brown film on the steel surface. ISSF marked 200-series grades as not recommended for food and beverage plant. Yet it reported positive experience with cutlery and cookware at 16% chromium or more.

Producers see a smaller gap. Jindal Stainless says 304 is only slightly better than its 200-series grades on pitting and crevice corrosion. It says every grade it tested lost less than 0.1 mm a year. That test ran for 720 hours in 3% salt water and mild organic acids. This is a producer claim. It also covers milder conditions than a wet prep counter.

No published test compares 202 and 304 under lemon juice, tamarind, vinegar or bleach. So there is no grade-specific figure for those. The general rule holds for every grade: acid and salt left standing on steel cause pitting. A chaat thela gets nimbu, imli and namak on its top all day. A dhaba sink gets wet masala and soap. Rinse surfaces and dry them at the end of each shift. The guide to maintaining kitchen equipment sets out daily cleaning routines.

How much more does 304 vs 202 stainless steel kitchen equipment cost?

Sheet 304 costs about ₹40–50 more per kg than 202. On published Indian price ranges, that is roughly 25–30% more. OfBusiness lists 202 at ₹140–170 per kg, 304 at ₹180–220 and 316 at ₹280–350. These ranges are undated and were read in Nov 2026. An imported 304 cold-rolled coil was listed ex-Delhi (the price at Delhi, before transport) at ₹2.20 lakh per tonne. A 201 coil was listed at ₹1.73 lakh (OfBusiness, about 12 Nov 2026).

Sheet and coil price ranges, India (OfBusiness, read Nov 2026)
GradePrice per kgIndex, 304 = 100
SS 202₹140–170≈75–80
SS 304₹180–220100
SS 316₹280–350≈155
SS 430not found–

For a finished table, the grade upgrade is smaller than sheet prices suggest. A 4 × 2 ft work table uses roughly 15–25 kg of sheet. So moving from 202 to 304 adds about ₹600–1,250 in material. This is an estimate from the per-kg gap, not a maker's figure. Labour, gauge (sheet thickness) and design move the final price more.

The budget ladder below shows where each buyer can start. A momo stall in Indore or a small cloud kitchen in Lucknow may buy one table first. A 30-seat restaurant needs several tables and a sink. A 100-cover hotel kitchen buys a full line. The rupee figures come from the prices above; they are not quotes.

Budget ladder: from a Starter stall to a full commercial kitchen
LevelWhat to buy and rough costWho it suits
StarterOne 202 work table or dry rack. 202 sheet costs ₹140–170 per kg. Listed 4 × 2 ft tables cost about ₹9,000–13,500; one 202 table was ₹10,800.A thela, momo stall or dhaba, for dry jobs: a packing table, utensil rack or kadhai stand
Small kitchen304 tops and sink, 202 frames and dry racks. A 304 top adds about ₹600–1,250 of material to a 4 × 2 ft table.A cloud kitchen, a 30-seat restaurant or a chaat counter with wet, salty tops
Full commercial304 throughout, at ₹180–220 per kg of sheet. 316 near the coast, at ₹280–350 per kg, about 55% more than 304.A 100-cover hotel kitchen; kitchens in Mumbai, Goa, Chennai or Kochi; pickle and seafood prep

At the Starter level, 202 is fine for a dry rack or frame. Spend on 304 for any top that meets nimbu, namak or water. Either way, ask for the grade in writing.

Can a magnet tell 304 from 202?

No. A magnet only separates ferritic steel, such as 430, from austenitic steel. Ferritic steel is the magnetic family with little or no nickel. 304 and 202 are both austenitic, and both are non-magnetic when annealed (ASSDA magnetic effects FAQ). If a magnet slides off a table top, the steel is not 430. It says nothing about whether the steel is 304 or 202.

Cold work confuses the test further. Cold work means bending, forming or drawing steel without heat. It turns part of the austenite into martensite, a magnetic form of steel. So a cold-worked 304 leg or tube can pull a magnet slightly, and 202 can do the same. Grades with more nickel, such as 316, resist this change. ASSDA also notes that magnetism says nothing about corrosion resistance.

How can you check the steel grade before you pay?

Three checks are reliable. A manganese drop kit is a quick screening test. A handheld XRF reading gives the full metal mix. XRF (X-ray fluorescence) is a handheld gun that reads metals using X-rays. A mill test certificate (MTC) is the steel mill's own record of the sheet's chemistry. A ₹300 kit sold by a New Delhi testing lab flags manganese, which marks 200-series steel. XRF reads chromium, nickel, manganese and molybdenum in 20–60 seconds without marking the surface.

Grade tests and their cost in India
TestWhat it showsCost
MagnetFerritic (430) or austenitic onlyFree
304/202 drop kitManganese present means 200 series; marks the surface₹300 per kit
Nickel kitIndication of nickel level₹700, about 200 tests
Molybdenum kit304 or 316₹650, about 300 tests
Spark testIndicative only; needs a grinder and practiceFree
Handheld XRFCr, Ni, Mn and Mo in 20–60 s; cannot read carbon or nitrogenNo current Delhi rate found
Lab analysisFull composition₹500 per element on one BIS lab scope
Mill test certificateThe mill's chemistry for that heat of steelFree from the supplier

Kit prices come from an IndiaMART listing by Advance Inspection & Testing Lab, New Delhi (undated). BIS is the Bureau of Indian Standards, the national standards body. The lab rate comes from one lab's scope on the BIS LIMS portal. NABL-accredited labs in Delhi NCR offer XRF. NABL is the national body that approves testing labs. None published a current per-sample price, so ask for a quote. A practical order of checks looks like this:

  1. Get the grade in writing, part by partThe top, undershelf, legs and sink bowl can each be a different grade. So the quote should name each one.
  2. Ask for the mill test certificateMatch the heat number on the MTC to the stencil on the sheet before fabrication. A heat number is the batch code of the steel. The stencil is usually cut off or polished away on finished goods.
  3. Rule out 430 with a magnetA strong pull on a flat panel means a ferritic grade, not 304.
  4. Run a drop kit on a hidden spotThe kit marks the surface. So test the underside of the top or the inside of a leg.
  5. Use XRF for large ordersA full kitchen of tables and sinks justifies a lab reading on each part. A stall owner buying one table can start with the ₹300 kit.

Weight is no help. Every stainless grade has a density of 7,700–8,000 kg per cubic metre (ASSDA). So a heavier table is thicker, not better alloyed. The same checks apply to second-hand kitchen equipment, where the original paperwork is often missing.

What gauge should a stainless steel work table be?

Gauge measures thickness, not grade. In India it is often given in SWG (Standard Wire Gauge). A lower SWG number means thicker sheet. A common build for a 4 × 2 ft work table is a 16 SWG top, an 18 SWG undershelf and 16 SWG legs. One listed 304 table at 48 × 24 × 34 inches had exactly that build at ₹9,800 (IndiaMART, undated).

UK Standard Wire Gauge (SWG) to millimetres (cutmy.co.uk)
SWGThickness
14 SWG2.03 mm
16 SWG1.63 mm
18 SWG1.22 mm
20 SWG0.91 mm

Measure at the sheet edge with a vernier calliper, a simple measuring tool. Don't rely only on the quote. US stainless gauges differ slightly: 16 gauge is 1.59 mm, against 1.63 mm for 16 SWG. So ask which system a figure uses, or ask for millimetres. A thin 304 top can dent and flex. A thick 202 top can still stain. That is why a quote needs both numbers.

Hadala two-burner commercial gas range in stainless steel

Hadala two-burner gas range

Listed in SS 304 with a 16 SWG top and an 18 SWG body. Grade and gauge are stated together, the way any stainless spec sheet should read.

View specifications

Where in a commercial kitchen does each grade fit?

SS 304 belongs wherever steel meets water, salt or food. That means prep tops, sinks, dishwash areas, hot wells and welded wet work. 202 can serve dry frames and racks. 430 suits outer panels. 316 earns its price in coastal and brine-heavy kitchens (Euro Inox; ASSDA; ISSF).

Use 304

Prep tops and work tables

Salt, masala, lemon and wet cloths sit on these surfaces all day. Stainless steel tables for restaurants should name 304 for the top. A chaat counter needs the same.

Use 304

Sinks and dishwash

These parts face constant water, detergent and welds at every corner. Dishwashing equipment needs 304 landing tables beside it.

Use 304

Hot wells and range tops

Hot water and spills reach these parts first. Hadala lists its bain marie counter in 304.

202 can work

Dry store racks and frames

Frames, side panels and undershelves for dry goods, kept rinsed and dry. Commercial stainless steel shelving for dry stores fits here. Racks in humid cold rooms still need 304.

Use 430

Outer panels and doors

Appliance bodies, doors and trims indoors. Because 430 is magnetic, it also suits induction cookware bases.

Use 316

Coastal and brine kitchens

Mumbai, Goa, Chennai or Kochi, pickle and seafood prep, and heavy chlorinated cleaning. Chloride, the salt in brine and bleach, can still crack 316.

Hadala bain marie counter with hot food wells
Hadala bain marie counterHot wells and counter tops meet hot water and spills first. So the grade matters most here.

The 202 split follows ASSDA's advice to keep chromium-manganese grades to milder conditions. It is a reading of the sources, not a published standard. Legs and bottom braces are the grey area. In most Indian kitchens they get wet during daily floor mopping. So 202 legs are a likely weak spot in a wet kitchen. No test data covers this case, though.

Here is how that looks at two sizes. A 30-seat restaurant can order 304 prep tops and sinks, with 202 frames for dry store racks. A momo stall or a Lucknow cloud kitchen buying one table should put 304 on the top first. A dry rack for packing boxes can stay in 202.

Dividing a kitchen into wet and dry zones makes the grade choice simpler. The guide to kitchen layout and space shows how to plan those zones.

Does Indian law require 304 for commercial kitchen equipment?

No. The Food Safety and Standards Authority of India (FSSAI) is the national food safety regulator. It requires equipment and containers that touch food to be corrosion-free, non-toxic and easy to clean and disinfect. But it names no steel grade (FSS Licensing and Registration Regulations 2011, Schedule 4, Part II, clause 3.1). An FSSAI directive of 15 June 2026 on corrosion-resistant knives restated the same rule.

A quality control order (QCO) is a government order that makes the BIS mark compulsory for a product. The cookware QCO of 15 January 2026 (S.O. 219(E)) made the BIS mark compulsory only for aluminium utensils and aluminium cans. Stainless steel utensils (IS 14756:2024) and sinks (IS 13983) were dropped from the final order (SGS, Feb 2026; Intertek, Jan 2026). So a stainless sink sold today need not carry a BIS mark.

In the United States, NSF/ANSI 51 is the standard for food equipment materials. It sets a 16% chromium minimum for stainless steel in food zones (2011 draft). Low-nickel grades such as J4, at about 15–16% chromium, can fall below it. For an Indian kitchen, 304 is best practice, not a legal requirement. It meets the corrosion-free rule with margin. The food licences and regulations guide covers the permits a kitchen does need.

What should a buyer ask for in a stainless steel equipment quote?

Ask for the grade and gauge of every part in writing, plus an MTC, before paying an advance. A quote that says only "stainless steel" lets the supplier use 202 or a lower-nickel grade on any part. It also gives the buyer nothing to test against. This holds for one thela table as much as for a hotel order.

  • Grade named separately for the top, undershelf, legs, frame and sink bowl, for example "top SS 304".
  • Gauge in SWG or millimetres for each part, such as a 16 SWG top and an 18 SWG undershelf.
  • Mill test certificate with a heat number that matches the stencil on the sheet.
  • Agreement to a drop-kit test on a hidden spot, or an XRF reading, before you accept delivery.
  • Clean welds with no brown or rusty discolouration. Such marks can point to sensitisation or poor pickling, the acid wash that cleans a weld.
  • SS 316 named for brine, pickle and seafood stations, or for kitchens near the sea.

With these six points in writing, any later argument about grade becomes a simple test against the quote.

What do kitchen owners ask about 304 and 202 steel?

Is 202 stainless steel safe for food contact?

Usually for dry, light use, but it is a weaker choice for wet food surfaces. ISSF reported positive experience with 200-series cutlery and cookware at 16% chromium or more. Yet it did not recommend these grades for food and beverage plant (ISSF, 2005). FSSAI names no grade. It requires surfaces that stay corrosion-free.

Does a magnet stick to 304 stainless steel?

No, not to flat annealed 304. Bent or formed parts such as legs and tubes can pull a magnet slightly. This is because cold work makes part of the steel magnetic. 202 behaves the same way, so a magnet cannot separate the two grades.

How can I check the steel grade at home?

A ₹300 manganese drop kit is the simplest home check. Manganese shows up strongly in 200-series steel and not in 304. Test a hidden spot, since the kit marks the surface. For a definite answer, ask for an XRF reading or a mill test certificate.

Is 304 worth the extra cost for a work table?

Usually, yes, for the top. On sheet prices, 304 adds roughly ₹600–1,250 of material to a 4 × 2 ft table. This is an estimate from the ₹40–50 per kg gap. It is about 4–14% of the ₹9,000–13,500 listed for 304 tables of that size. A small stall can still use a 202 frame under the 304 top.

When should a kitchen choose 316 over 304?

Usually only near the sea or for brine-heavy work. Euro Inox recommends 316 for salty or aggressive foods and brines. So coastal kitchens and pickle or seafood prep gain most. Sheet 316 costs about ₹280–350 per kg, roughly 55% more than 304.

Does a BIS mark prove a stainless sink is 304?

No. The January 2026 quality control order dropped stainless steel sinks (IS 13983) and utensils from compulsory BIS marking. So a sink need not carry the mark at all. Ask for the grade in writing and a mill test certificate instead.

Keep reading

More kitchen guides

See all blogs

Plan your kitchen the smart way

See the full equipment range, or start with a guide and work out the costs first.

EquipmentGuidesPartner